Hi,
I'm wondering if someone is using a pad (and what kind of pad, eg. silicone, rubber, etc...) to press boards with 3D core. I tried with a rubber pad between the top of the layup and the top cassette but the pad is not enough firm so I have imperfections on the top of the board. I can't find a pad that is firm enough to get a perfect finish and soft enough to conform to the 3D shape of the core. any help will be appreciated.
Pressing with a pad
Moderators: Head Monkey, kelvin, bigKam, skidesmond, chrismp
-
- Posts: 181
- Joined: Tue Jul 07, 2009 4:41 pm
- Location: Southern NH
- MontuckyMadman
- Posts: 2395
- Joined: Fri Jun 20, 2008 9:41 pm
I would contact one of the many RTV or silicon rubber manufacturers and explain your pressure and application. they will send you different durometer samples of cured rubber and you can test small samples.
Smooth-on makes allot of mold rubber this is used in the mold injection industry, hot wax investment casting for art and science and movie making and architectural.
http://www.smooth-on.com/
I'm thinkin shore a 60? or so pretty hard. Depend on what your shape is.
http://en.wikipedia.org/wiki/Durometer
Most likely from the samples you can determine what duromter works best for your application. Post your results here please.
Smooth-on makes allot of mold rubber this is used in the mold injection industry, hot wax investment casting for art and science and movie making and architectural.
http://www.smooth-on.com/
I'm thinkin shore a 60? or so pretty hard. Depend on what your shape is.
http://en.wikipedia.org/wiki/Durometer
Most likely from the samples you can determine what duromter works best for your application. Post your results here please.